NEXUS Send drawings
MANUFACTURING GUIDE / 08

6061 or 7075 aluminium: choosing the grade.

Grade selection is an engineering decision, not a purchasing preference. The comparison below covers the points that change a machining route — strength, stability, finishing and distortion.

What actually differs between the two grades

6061 (magnesium-silicon) offers moderate strength, good machinability, corrosion resistance, predictable anodising and real weldability. 7075 (zinc-magnesium-copper) delivers much higher strength — the aerospace pick — with lower corrosion resistance, stress-corrosion-cracking risk and no practical weldability.

Where strength stops being the deciding factor

Parts usually fail from stress concentrations, thin-wall deflection or datum shift — not from a slightly weak alloy. Fix geometry first: fillets, wall thickness, corner radii. Upgrading to 7075 to rescue a bad profile buys cost, not margin.

Machining behaviour and distortion

7075 cuts cleanly but is less forgiving of heat and residual stress; thin sections can move. The published thin-wall case achieved flatness ≤ 0.05 mm on 6061-T651 (426 × 221 × 36 mm) through rough machining, stress relief and finish milling with temporary supports — the same discipline matters more on 7075.

Corrosion, anodising and coating consequences

6061 anodises predictably. 7075's copper and zinc content complicates both corrosion behaviour and anodised appearance — finish specifications should be reviewed together with the grade choice.

Cost and supply reality

7075 costs more and stock is narrower by thickness and temper. State whether equivalent grades are acceptable, or the RFQ dies in procurement.

Grade selection: the questions that decide it

Requirement60617075
Strength-to-weightAdequate for enclosures, covers, bracketsPreferred when high strength governs
DistortionGood stability, predictable after stress reliefHigher residual stress; thin sections need care
Corrosion / finishGood, predictable anodisingLower resistance; review finishing together
WeldabilityWeldableNot practically weldable
Cost / availabilityLower cost, wide stockHigher cost, narrower supply

What to put on the drawing and RFQ

Name the alloy and temper (6061-T651, 7075-T6), state whether equivalents are allowed, flag the critical surfaces, and send the 3D model, 2D drawing, quantity and finishing/inspection requirements together.

START WITH YOUR DRAWING

Turn the guide into a quotation.

Chat on WhatsApp